An eVTOL battery cold plate is best built as an extruded multi-channel aluminum core joined by brazing, with CNC used only for local features. Machining a 1.3-meter-class thin plate from solid removes too much material, distorts the part and adds weight. The route below comes from a real engineering review and DFM we completed for an electric-aviation developer.


An electric-aviation (eVTOL) developer needed a battery heat exchanger for a cylindrical-cell pack. The part is a 1.3-meter-class, thin-wall aluminum plate with multiple internal channels and a functional insulation coating. It is a thermal part, a pressure part and an electrical-insulation part at the same time, so standard industrial cold plate practice does not apply.
Customer requirements included:
| Parameter | Customer requirement |
|---|---|
| Coolant | 50/50 water–glycol, design flow about 12 L/min |
| Pressure drop | Low-resistance target; 1 bar maximum |
| Pressure validation | 3 barg working, 4.5 barg proof, 9 barg burst |
| Helium leak rate | ≤ 5 × 10⁻⁷ Pa·m³/s |
| Flatness (contact zone) | 0.1 mm within any Ø20 mm area |
| Insulation coating | 250 µm ± 50 µm; Hi-Pot at 4 kV |
| Environmental references | Aerospace test standards such as DO-160G (thermal cycling, vibration) |
We recommended an extruded multi-channel core joined by brazing, rather than deep-milling the whole plate from solid. Full CNC removes too much material, distorts long parts and adds weight; we kept CNC for local features only. We also compared brazing with friction stir welding (FSW): FSW would have required more frame material and a redesign of the seam path, so it was not the first choice for this geometry.

The DFM mapped every step — extrusion, cutting and end machining, cleaning, brazing, post-braze flattening, leak and pressure testing, coating, masking of grounding areas, and final inspection — with the main risk at each step: flatness on a long thin plate, channel consistency, braze stability, port and manifold reliability, and coating thickness versus thermal resistance.
Helium mass-spectrometer leak testing per part, proof and burst testing, a full ΔP–flow curve (not a single point) on a water–glycol rig, Hi-Pot and adhesion checks after coating, free-state and constrained flatness, weight logging and automated CMM inspection, all with serial-number traceability.


| Control | Value / method |
|---|---|
| Base material | 3003 aluminum, extruded multi-channel profile |
| Thin-wall zones | 1.5 mm walls, included in the coating coverage zones |
| Pre-braze cleanliness | 38 dyne pen test: line ≥ 100 mm, read at 2.0 ± 0.5 s; pass only if the line stays continuous with no beading |
| Brazing | Furnace temperature checked against the target profile and recorded before every run |
| Post-braze flatness | Press reshaping to 0.1 mm within any Ø20 mm area of the contact zone |
| Leak test | Dual-chamber helium mass spectrometer; ≤ 5 × 10⁻⁷ Pa·m³/s |
| Coating thickness | 250 µm ± 50 µm, including internal corners, fitting interfaces and insert edges |
| Dielectric test | 4 kV, 10 mA, 1 minute; no breakdown allowed |
| Coating adhesion | Cross-hatch test |
| Grounding areas | Masked before coating; must remain electrically conductive |
| Dimensional release | Full-dimensional automated CMM inspection before shipment |
No thermal or pressure-drop test results are published yet: the project is at the DFM stage, and those values will be measured on prototypes.
We did not choose additive manufacturing as the first route: it suits small, complex parts, but at this length the build envelope and cost per part were the limiting factors.
| Process step | Main risk we controlled |
|---|---|
| Extrusion of multi-channel core | Channel consistency along the full length |
| Cutting and end machining | Port geometry and burr control |
| Cleaning | Residues that affect braze quality |
| Brazing | Joint stability, filler flow into channels |
| Post-braze flattening | Flatness on a long, thin plate |
| Leak and pressure testing | Port and manifold reliability |
| Insulation coating | Thickness versus thermal resistance |
| Masking of grounding areas | Electrical contact zones left uncoated |
| Final inspection | Traceability by serial number |
Engineering review and DFM completed; a staged prototype path (structure → leak and pressure → coating → thermal) has been defined with the customer.
Related: eVTOL battery liquid cold plate manufacturing guide
Have a long, thin or coated battery cold plate to evaluate? Send your drawing — an engineer reviews every RFQ and replies by email with next steps.
Send Your Drawing →